Blanking of forgings: bars with diameter>40mm are mostly cut by circular saws, and bars with small diameter can be cut by grinding wheels. When the requirements are high, the lathe can be used for blanking. If there are scratches and other defects on the surface of martensite raw materials, they need to be peeled by lathe or grinded by centerless grinding.
Heating of forgings: electric furnace or flame furnace can be used for heating before forging. Flame furnace is widely used in production. For austenitic stainless steel, the furnace gas shall be kept neutral or slightly oxidizing to avoid intergranular corrosion caused by carburization; For martensitic stainless steel, excessive oxidation atmosphere cannot be used to avoid serious decarburization.
Under 700~800 ℃, the thermal conductivity of stainless steel is relatively small, so the heating time required for forging stainless steel forgings is longer. When ferritic stainless steel is heated to high temperature, the grain growth tends to be serious, resulting in greater brittleness. The oxidation and decarburization of martensitic stainless steel are particularly serious at high temperature. They all require to shorten the heating time at high temperature as much as possible. Therefore, these two types of steels, as well as austenitic stainless steel with diameter or thickness exceeding 100mm, generally adopt two-stage heating: first slowly heating to 850 ℃, and then rapidly heating to the initial forging temperature.
For the blank directly put into the high-temperature furnace for heating, the heating time shall be calculated as 2 mm/min from the time of entering the furnace; For the blank heated in two stages, the preheating stage time is calculated as 2 mm/min, and the heating time in the later stage is calculated as 3 mm/min.
For precision forgings or important forgings with small allowance, a layer of glass lubricant shall be coated on the blank surface before heating, and then heating. The glass lubricant is generally prepared with 57% glass, 3% clay and 40% water.
Stainless steel with high nickel content must be heated with sulfur-free fuel. Because sulfur penetrates into the steel and forms low melting point sulfide with nickel and eutectic is distributed on the grain boundary, intergranular cracks will occur during high temperature forging.
Jan 28, 2023
Blanking and heating of forging